Equipment

The coatings are deposited in three professional systems:

nanasanje
coatings

CemeCon CC800/9
CemeCon CC800/7
Balzers BAI730

We use the following deposition techniques:
evaporation
sputtering
pulsed sputtering

Coating thickness: 2–3 μm for cutting tools, 3–5 μm for forming tools

Basic requirements:
correct surface preparation
the deposition temperature is 450 °C
CrN and TiN can also be prepared at 200 °C
maximum tool size   Ø 400 mm x 400 mm


We posses the most modern techniques for surface and thin film analytics:

analysis
analysis

electron microscopy
optical microscopy
mechanical tests (hardness, adhesion, wear)
corrosion tests
chemical analysis

In addition to coating deposition, we also offer:
designated professional seminars
consulting in industrial implementation of coatings
investigations and expert opinions
application of joint projects (national and international)