Equipment
The coatings are deposited in three professional systems:

CemeCon CC800/9
CemeCon CC800/7
Balzers BAI730
We use the following deposition techniques:
– evaporation
– sputtering
– pulsed sputtering
Coating thickness: 2–3 μm for cutting tools, 3–5 μm for forming tools
Basic requirements:
– correct surface preparation
– the deposition temperature is 450 °C
– CrN and TiN can also be prepared at 200 °C
– maximum tool size Ø 400 mm x 400 mm
We posses the most modern techniques for surface and thin film analytics:

– electron microscopy
– optical microscopy
– mechanical tests (hardness, adhesion, wear)
– corrosion tests
– chemical analysis
In addition to coating deposition, we also offer:
– designated professional seminars
– consulting in industrial implementation of coatings
– investigations and expert opinions
– application of joint projects (national and international)